- High thermal conductivity up to 7.0 w/mºk , low thermal resistance of 0.01°C-In2 /W
- Low viscosity & excellent wetting properties allows screen printing/Stencil method to apply precise bond line thickness.
- Available in Non Silicone, Silicone and high temperature (up to 360°C) formulas